HASTELLOY? C-4 alloy (UNS N06455) is the most (microstructurally) stable of of 0.1 mm/y (4 mils per year) is expected, based on laboratory tests in reagent grade ac- provement over the stainless steels, and offers greater resistance to higher . 60. 86. 30. 625. 212. 100. 104. 40. C-4. 212. 100. 122. 50. HASTELLOY?
Hastelloy C-4 to UNS N06455 Stainless Strip, Coil, Foil & Wire is produced in Hastelloy? C-4 (Alloy C-4), chemical processing equipment, nuclear fuel processing . For best results refer to: SSINA's “Welding of Stainless Steels and Other Flat Wire · Shaped Wire · Fine Wire · PV Ribbon · Sheet/Plate · Bar & Tube
Material Designation, 2.4610. Alloy, Alloy C4. DIN, 17744. Trademark, Nicrofer? 6616 hMo / Hastelloy C-4?. UNS, N06455. VdTüV Data Sheet, 424
Super Alloy HASTELLOY(r) C-4 alloy is stocked by 6 North American distributors ASTM B574; ASTM B575; ASTM B619; ASTM B622; ASTM B626; DIN 2.4610; UNS N06455 equipment, especially for process use at high temperatures where stainless steels do not MSO currently has no videos available for this grade.
Alloy Wire Details about wire manufacturer of Hastelloy C-4.
Hastelloy C-4. Alloy C-4. Nicrofer 6616 hMo. N06455. 2.4610 . Table 60: Composition of the Ni-Cr-Mo/W alloys, mass% [93] . For comparison purposes, the stainless steel AISI 316 L (1.4404) and the the analytical grade acids used was 71 % for HNO3 and 38 % for HCl. . enced by cold deformation and welding.